Solution for removing copper ion impurities from nickel solution


Release Time:

Oct 25,2013

1. Reasons for black spots in traditional nickel plating
In the gravure printing industry, the nickel plating solution has a high concentration of copper ions and chloride ions in the nickel plating tank, which can lead to the reduction of copper ions on the cathode surface and the potential formation of cuprous chloride. The formed cuprous chloride can adsorb on the cathode surface. Due to the high hydrogen evolution potential of cuprous chloride, hydrogen evolution occurs on the cuprous chloride particles during the electroplating process, causing the pH to rise. The pH of the nickel plating solution is close to neutral, making it easy to reach the pH value that forms metal precipitates. When metal ions (mainly nickel ions) reach this area, precipitates will form and be mixed into the plating layer, resulting in black spots.

The formation of black spots on the nickel plating layer severely affects the quality of the subsequent copper plating layer, making the polishing of the nickel plating layer an essential process. For a long time, the polishing of the nickel plating layer has restricted the advancement of production automation and wasted labor and raw materials.

 

2. Main measures to achieve clean plating solution
1. Add copper removal agent
2. Nickel plating additives
3. Electrolytic cell device
4. Standardize process parameters
5. Ensure the roughness of the plate roller and clean thoroughly


Method 1: Use a copper removal agent to remove most of the copper ions
Steps:
Add a quantitative amount of copper removal agent to the plating solution, which forms characteristic precipitates with copper ions, effectively removing most of the copper impurities in the nickel plating solution and improving the quality of the plating layer.
After adding the copper removal agent, it needs to be stirred evenly and the filter machine should be turned on to filter for about 3 hours.


Method 2: Add nickel plating additives during production
1. Nickel additives are chelating agents that can form chelates with copper and iron ions.
2. They can change the deposition potential of copper and iron ions, making the electrode potential of impurity ions close to that of nickel ions.
3. Impurity ions and nickel are simultaneously deposited on the cathode, avoiding burrs in the plating layer.


Method 3: Continuous electrolysis to remove copper ions using an electrolytic cell device
During production, the introduction of copper ions is continuous, and controlling the copper ion content is crucial. Continuous control is needed during production. To avoid the inconvenience of using electrolysis or adding copper removal agents to control copper ion content, an electrolytic device can be installed outside the plating tank to allow copper ions to be continuously electrolyzed out.
The electrolytic cell is compact, has very low energy consumption, and facilitates impurity cleaning. It plays a significant role in production and can effectively reduce the amount of copper ions introduced into the nickel tank during production.

 

4. Standardize nickel plating process parameters

5. Ensure the roughness of the plate roller and clean thoroughly
1. Ensure the roughness of the plate roller is within 1±0.1um.
2. After cleaning and polishing, the roughness should be within 0.7±0.1um, the plate surface must be thoroughly degreased, and rust must be cleaned off.
3. After cleaning, it should be placed in the tank in a timely manner to avoid prolonged storage.

Leave Messags.